Hi Werner,
Are you referring to the differing thermal coefficients contributing to
unreliability?
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Thursday, August 26, 1999 6:02 AM
To: [log in to unmask]
Subject: Re: [TN] Advice on solder pad design
Hi Eric,
Get a copy of IPC-SM-782.
But why are you considering LCCs (leadless ceramic chip carriers)? Are you
mounting them on ceramic? If you are using FR-4 or any other polymer-based
substrates you can forget about reliabilty in any environment other then a
really benign one, such as sub-ocean cable repeaters. You could of course
put
solder columns on the component.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|