Nick,
If your PWB finish is HASL it might not make a lot of sense. If it happens to
be OSP it makes a lot of sense as OSP in not conductive and I understand
it tends to cause problems with test probes.
We use OSP and I have added our test points to the solder stencil for this very
reason.
DT
At 02:58 PM 8/25/99 -0400, you wrote:
>On double reflow boards our ICT test engineers now want to solder paste the
>solder side test points prior to reflow. We do not see any advantage to this
>but about 2000 more holes in the stencil. What are your ICT people saying.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################