* FR-4 is "the" expression used by NEMA (National Electrical
Manufacturers Assiociation, USA) in their standard LI-1.
* NEMA LI-1 and MIL-P-13949 (now replaced by IPC-4101) are similar
(but not exactely identical)
* FR-4 conforming NEMA LI-1 equals to GF conforming MIL-P-13949
* "FR" means also flame retardant.