In a message dated 07/02/1999 1:04:59 PM US Eastern Standard Time,
[log in to unmask] writes:
>
> Now,
> I need to create a plan to qualify a new process for use on an existing
> product. Does anyone have any pointers on how to go about doing this?
What
> we are trying to do is switch from hand soldering a product line to wave
> soldering as much as possible on the same product line. Our customer has
> given us the green light as long as we qualify the process.
Eric,
When you say "qualify" a process, it begs the question "to what standard or
specification"? Will you be using internal company standards? J-STD-001?
Revision A? Revision B?
When you answer this question, I can be of more help.
Doug Pauls
CSL