TECHNET Archives

July 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Earl Moon <[log in to unmask]>
Date:
Mon, 5 Jul 1999 12:38:02 -0500
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (13 lines)
We use no flux when preparing a rework site, after BGA removal, and all pads
look and rework fine. We ocassionaly replace and reflow BGA's without solder
paste using our choice of paste, not liquid, flux. This too works fine and
X-Rays (always used after BGA rework) show no voiding.

Mostly, we replace and reflow BGA's using solder paste. We also use high temp
solder balls in each of four corners to effect real solder fillets much as
with column grid arrays as our data shows them to be more reliable.