Dave: True the copper and gold will diffuse, however the copper overplate is
about 1000 - 1500U" thick over the gold. At that thickness of copper it does
not create any solderability problems.
Again this copper overplate is typically only on the vias and their pads
that are located in the gold feature areas.
The active contact surface for the switch, touch pad, etc. is gold over
nickel and not soldered to. This was the area that was masked off during the
copper pattern/over plate operation. A little hard to visualize, I know
without a picture.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
425-356-6076
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Wednesday, July 28, 1999 7:29 PM
To: TechNet E-Mail Forum.; Barmuta, Mike
Subject: Re: [TN] NI/AU UNDER BETWEEN COPPER
Hi Mike - I have a question! My experience has been that the copper and
gold will diffuse together to form a stable alloy which is very (but not
impossible) hard to solder. In the application you describe, is this final
copper/gold surface the contact surface for the switch, touchpad, etc. and
not a surface that gets subjected to a soldering operation?
Dave Hillman
Rockwell Collins
[log in to unmask]
"Barmuta, Mike" <[log in to unmask]> on 07/26/99 05:19:30 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Barmuta, Mike" <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] NI/AU UNDER BETWEEN COPPER
Susan: We have built product similar to this using a process called
"Selective First Gold". The Ni/Au feature(keypad, LCD pad, rotary switch
etc,)is plated directly onto the electroless Cu. Sometimes these Au
features
contain vias which require a full build up of plated Cu in the hole. To
accomplish this the Au feature is covered with plating resist except in the
via area where it is opened up with a pad and overplated with Cu during the
primary circuit Cu pattern plate operation.
The cross section of the finished hole would be: els Cu 50u", Ni
electroplate 200u", Au electroplate 25u", Cu electroplate 1200u".
We have not experienced any reliability issues for these products based on
this style of construction.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
425-356-6076
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, July 26, 1999 8:20 AM
To: [log in to unmask]
Subject: [TN] NI/AU UNDER BETWEEN COPPER
I just looked at a product where the manufacturer has managed to
overplate nickel/gold with copper. This occurs on the surface conductors
and also in holes.
I have looked in the design and board documents, but cannot find anything
that addresses the reliability of such a condition. I know putting a
"meltable"
material between layers of copper can wreak havoc, but what about
ni/au?
Susan Mansilla
Robisan Lab
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|