I also have heard that this alloy suffers from oxidation and embrittlement
problems.
-----Original Message-----
From: Andy Mackie <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Wednesday, July 07, 1999 11:12 AM
Subject: [LF] Tin / Zinc
>Just from its melting point (198.5°C), the approximately 91Sn/9Zn eutectic
seems
>to be an ideal alloy for soldering, although the zinc seems to make the
alloy
>prone to corrosion (much like the lead-phase in Sn/Pb) in solder pastes,
and it
>gives excessive drossing in wavesoldering.
>
>I've heard that the zinc phase is a problem AFTER processing, too, but have
>never seen any actual documentation of this: is this a technomyth, or does
>someone out there have evidence of post-assembly corrosion?
>
>Toodle pip,
>
>Andy Mackie
>
>################################################################
>Leadfree E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask]
>with following text in the body:
>To subscribe: SUBSCRIBE Leadfree <your full name>
>To unsubscribe: SIGNOFF Leadfree
>################################################################
>IPCWorks -October 25-28 featuring an International Summit on Lead-Free
Electronic
>Assemblies.
>Please visit IPC's Center for Lead-Free Electronics Assembly
>(http://www.ipc.org/html/leadfree.htm ) for additional information.
>For technical support contact Gayatri Sardeshpande [log in to unmask] or
847-790-5365.
>################################################################
>
################################################################
Leadfree E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask]
with following text in the body:
To subscribe: SUBSCRIBE Leadfree <your full name>
To unsubscribe: SIGNOFF Leadfree
################################################################
IPCWorks -October 25-28 featuring an International Summit on Lead-Free Electronic
Assemblies.
Please visit IPC's Center for Lead-Free Electronics Assembly
(http://www.ipc.org/html/leadfree.htm ) for additional information.
For technical support contact Gayatri Sardeshpande [log in to unmask] or 847-790-5365.
################################################################
|
|
|