-----Original Message-----
From: Tempea, Ioan [mailto:[log in to unmask]]
Sent: Friday, July 09, 1999 12:18 PM
To: [log in to unmask]
Subject: [TN] PCB blistering during wave
Fellow technetters,
we are presently fighting with some ultra low-end TH only PCBs. During
waving they blister a lot. We tried many things like hotter-colder
preheating, hotter-colder solder temp, faster-slower speed. No result.
Are there any other tricks to try, or we send them back to the fab?
Thanks, Ioan
|
|
|