Hi Kathy,
You have my sympathies; when people in the same company work at
cross-purposes you can expect nothing but trouble.
I certainly have no idea what 'evidence' your Purchasing people will consider
being adequate, given the evidence you already have. However, perhaps you
need failed solder joints to convince them. Just cross-sectioning your SJs
with inadequate wetting will not convince them (given your statements), but
if you take some of the assemblies made (under protest as you state) and
T-shock them 25C<->110C, your product excursions, for about 30 cycles (they
are likely to fail much earlier), you would get some beautiful (?) fractured
solder joints showing failure at the interface in the absence of a
metalurgical bond (intermetalic compounds).
If that does not convince them, nothing will.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|