Hi Jim,
As far as I know, some bar solder manufacturers make a "high-purity" solder
bar as well as a "normal" bar. If you are running the "normal" bars, mixing
in a high purity bar probably wouldn't hurt. On the other hand, if you are
running "high purity" bars, and you add normal bars, you might be
contaminating your bath.
"West, Jim" <[log in to unmask]> on 07/28/99 03:40:16 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "West, Jim" <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Charles Barker/US/I-O INC)
Subject: [TN] Mixing solder bars from different
manufacturer's
Hi all,
This might be a silly question, but I received some left over solder from a
customer that is made by a different manufacturer than what we use. Both
solder bars are 63/37 and I want to know if you can mix solder from
different manufacturers, I'm not sure if manufacturers do anything
different
with their product or if any quality issues could arise.
Thanks,
Jim West
Manufacturing Engineer
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|