My understanding of the usual oxide removal procedure is a 3-minute soak with 5%HCl. The goal is a very mild etch, and I've heard that nitric acid will cause pitting instead - and this is in line with some laboratory oxidation studies I did some time ago. Variability in solderability data was much higher on aged coupons I had treated with dilute HNO3 than on coupons treated with 5%HCl.
LeRoy
-----Original Message-----
From: nishath yasmeen [SMTP:[log in to unmask]]
Sent: Friday, July 23, 1999 3:34 PM
To: [log in to unmask]
Subject: [TN] Copper oxide removal
Hello everyone!
Is Nitirc acid ( dilute) a better acid than sulfuric for cleaning
the oxide on plated copper?
Any information provided will be appreciated.
Yasmeen
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|