My wave solder stiffeners are all Titanium. Stainless steel also works
well. Joe
At 01:28 PM 6/11/99 +0100, you wrote:
>We are currently manufacturing a new production line which uses carriers
>which traverse around a moving line for assembly prior to going over a wave
>soldering machine.
>
>The problem is the carriers are made of an FR4 type material but what
>material can be used as stops on the underside of the carriers to stop wear.
>The tool maker has tried metal stops (steel) but these pick up solder. Even
>stainless steel causes problems because a film of solder picks up on stop
>and causes problems when it falls off on the line.
>
>
>Thanks,
>
>Neil Atkinson
>Quality Manager
>Stadium Electronic Controls
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
Joe Wackerman
Sr. Mechanical Engineer
Parker Hannifin
Compumotor Division
5500 Business Park Drive
Rohnert Park, CA 94928
http://www.compumotor.com
voice 707-584-2522
FAX 707-584-8015
e-mail [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|