In a message dated 06/11/1999 2:48:37 PM US Eastern Standard Time,
[log in to unmask] writes:
> What does the industy do for qualifications and reliability for BGAs? What
> testing is generally done. I'm trying to see if a BGA connection is
> affected in any way by going through the wave solder for qualifying that in
our process.
> Any insight would be helpful.
Whenever the word "qualification" is used, it begs the question
"Qualification to what standard"? To my knowledge, there is no IPC (or other
organization) that specifically covers qualification of a BGA attach process.
J-STD-001, revision B, when modified with a little engineering insight and
use of a suitable test vehicle, could be used. Do you have internal
workmanship standards or quality control provisions that your are trying to
meet?
Doug Pauls
Technical Director
CSL
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|