I used to be involved in printing ceramic hybrids and we used to 'print' the
conductive inks through the holes. The ink was printed over the holes and
then a vacuum was used to pull the ink through the holes. This was done on
both sides of the ceramic tile to ensure that there was a good connection
between both sides. This operation was always the first print to be carried
out.


===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
7/06/99 03:51
>Hi
>
>Can anyone provide me some infomation regarding through hole metalization
>for ceramic materials? Is that similar to the electroless Cu or direct
>metalization process for PWB material such as FR4?
>
>Thanks
>Li Kang
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
>################################################################


Mark Austin (Process Engineer)
ACW Technology Limited
Hylton Road
Petersfield
GU32 3XX
ENGLAND

TEL - +44 (0) 1730 300000
FAX - +44 (0) 1730 266045

Email - [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2