Our Engineering depatment is doing some temperature cyclying and vibration
testing (HALT type testing). Can any or you tell where I can get reference
material about the effect this has on the solder joints? Some of the
variables I would like to become knowledgable about are: component height
and mass, joint design, solder alloy variations, effect of reflow profile,
etc.

We will probably be testing over a temp range of -60 to -65  C up to the
neighborhood of +125 C or thereabouts and shock maybe up to 40, 50 or 60
g's.

Are there any "programs" or formulae readily available which will predict
joint failure after so many cycles at certain temps, freqs, and g's?

TIA

Charlie Barker

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2