In a message dated 06/10/99 9:28:41, [log in to unmask] writes:
> Can anyone tell me what the minimum tin/lead plating thickness should
> be inside a plated through hole?
Hi David,
You did not say whether you are talking about PTHs or PTVs (vias).
For PTVs, there is no need for any tin/lead plating.
For PTHs, into which you want to solder component leads, the tin/lead plating
thickness will provide some protection to preserve the solderability of the
underlying copper, but you need to consider that tin/lead plating is porous,
and thus not very good at this job. Thus, tin/lead plating typically is
reflowed. To get good solderability shelf life you need about 5 micro-meters
of solder; on the other hand, there is no critical need for having good
solderability inside a PTH barrel. Thus, there is no industry standard on this
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|