Solution: Use Locktite X-NMS Cleanup Solvent #76820, MEK can wrinkle/shrivel or dissolve into a slime, some mask materials
X-NMS is great for cleanup of Tak-Pak products, or any "Super-Glue" based adhesive, whether in the cured or uncured state, but preferably in the cured condition.
Ron Leckfor
QC Coordinator
REM Electronics Supply - Value Added Division
Warren, Ohio
330 373 1300 X 240
http://www.remelectronics.com
-----Original Message-----
From: Tempea, Ioan [SMTP:[log in to unmask]]
Sent: Wednesday, June 02, 1999 1:39 PM
To: [log in to unmask]
Subject: [TN] Fingerprints II
Thanks a lot everybody for the strong response to my problem.
Now I know this is a common problem and I fixed it with gloves.
The problem number two is that I, however, have 20 assemblies that could
serve in a criminalogy teaching class. Is there any way to clean them? I
tried several substances I had around and Methyl Ethyl Ketone works the
best. Will it damage the board (solder mask, joints, ICs, etc)?
Thanks, Ioan
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|