TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Stillings <[log in to unmask]>
Date:
Tue, 15 Jun 1999 11:49:10 -0400
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Stillings <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Hi technetters,
Hope all is well.....................  Got a quick question - I am using Power
chip resistors (manufacturers name with held :) ) that have a "solder plated
phosphor bronze" terminal.  I am having a bugger of a time soldering these
parts.  I have limited solderability testing capabilites and am forced to use
the old solder pot test to verify solderability.  I get good solder adhesion on
some and very poor on others.  I don't have any experience with phosphor bronze
based terminals.  I am looking for your expertise on how I can wave these parts.
Note:  leads are very dark in color as if they are contaminated but the date
codes on the parts is very new. Oh yeah - sodler is 63/37 with no clean alcohol
base flux spray.

Thanks again in advance for the help!

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2