Typically we use titanium. It works very well. Give me a call and I'll fill
ya in. If you are using a no clean flux though, almost any material will
after numerous passes build up a film and then solder sticks to the film,
not the metal.
Jim Gleason
972-494-1911
-----Original Message-----
From: Neil Atkinson <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, June 11, 1999 9:29 AM
Subject: Re: [TN] Carrier Materials
>> -----Original Message-----
>> From: Neil Atkinson
>> Sent: 11 June 1999 13:28
>> To: 'IPC Technet'
>> Subject: Carrier Materials
>>
>> We are currently manufacturing a new production line which
>> uses carriers which traverse around a moving line for
>> assembly prior to going over a wave soldering machine.
>>
>> The problem is the carriers are made of an FR4 type material
>> but what material can be used as stops on the underside of
>> the carriers to stop wear? The tool maker has tried metal
>> stops (steel) but these pick up solder. Even stainless steel
>> causes problems because a film of solder picks up on stop and
>> causes problems when it falls off on the line.
>>
>>
>> Thanks,
>>
>> Neil Atkinson
>> Quality Manager
>> Stadium Electronic Controls
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|