TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Neil Atkinson <[log in to unmask]>
Date:
Fri, 11 Jun 1999 15:05:24 +0100
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Neil Atkinson <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
> -----Original Message-----
> From: Neil Atkinson
> Sent: 11 June 1999 13:28
> To:   'IPC Technet'
> Subject:      Carrier Materials
>
> We are currently manufacturing a new production line which
> uses carriers which traverse around a moving line for
> assembly prior to going over a wave soldering machine.
>
> The problem is the carriers are made of an FR4 type material
> but what material can be used as stops on the underside of
> the carriers to stop wear?  The tool maker has tried metal
> stops (steel) but these pick up solder.  Even stainless steel
> causes problems because a film of solder picks up on stop and
> causes problems when it falls off on the line.
>
>
> Thanks,
>
> Neil Atkinson
> Quality Manager
> Stadium Electronic Controls

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2