> Magic Solder ???
>
> Tacking modification wires to PCB. We were once able to purchase a product
> marketed as Magic Solder, it is a glue stick that can be melted using a
> soldering iron tip then used to secure the modification wire to the PCB
> surface.
>
> Can anyone help with a contact for this or a similar product? Or
> recommended any alternative simple techniques for tacking modification wire
> to the PCB surface?
Not heard of this product, but would like to know more...
Some other options!
1) PRELEG wire is a ptfe mod wire with a pre-deposited hot melt adhesive, which
you apply with a grooved soldering iron tip. Sounds like a more sophisticated
version of what you asked for. Preleg are in Englewood, Florida.
2) There are *very* fast light cure wire tacking adhesives available now, which
can use cheap spot lamps to cure. Try Dymax, Loctite.
3) Self adhesive dots with a very high tack adhesive.
I wrote an article about this once, which, unfortunately, is not on-line. But I
would be pleased to *fax* it to anyone who e-mails me their fax number, off
TechNet.
Peter
--
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
Peter Swanson Oxfordshire, England
INTERTRONICS
[log in to unmask] http://www.cygnetuk.demon.co.uk
Suppliers of materials and consumables to the electronics & related industries
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|