TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Joe Felts <[log in to unmask]>
Date:
Tue, 1 Jun 1999 14:13:57 -0700
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Joe Felts" <[log in to unmask]>
Parts/Attachments:
text/plain (78 lines)
FR4
Tensile Strength
        Lengthwise (warp direction?):   40,000 psi
        Crosswise:                      35,000 psi
Compressive Strength
        Flatwise:                       60,000 psi
        Edgewise:                       35,000 psi
Flexural Strength (1/8 in. thick)
        Lengthwise:                     55,000 psi
        Crosswise:                      45,000 psi
Modulus of Elasticity in Flexure
        Lengthwise:                     2.7 Mpsi
        Crosswise:                      2.2 Mpsi
Shear Strength                          19,000 psi
Izod Impact, (ft-lb/in of notch)
        Flatwise                        7
        Edgewise                        5.5

No fatigue data.
Source: Modern Plastics Encyclopedia 1986-1987.
If you can get your hands on a later version, you may get some better data.

Joe Felts


-----Original Message-----
From:   PAUL BROWN [SMTP:[log in to unmask]]
Sent:   Monday, May 31, 1999 8:00 AM
To:     [log in to unmask]
Subject:        [TN] Under Stress

Hi all,

We are currently modeling the response of some of our PWB's to flexure.
One issue which keeps presenting itself is a lack of a good sources for
the mechanical properties of standard high temp FR4/ copper laminate
boards. Although I realize that such properties are stack-up specific,
does anyone have or know of a ranges for these properties. Of interest
would be: modulus of elasticity (in X, Y, Z), Ultimate tensile strength
(UTS), Ultimate shear stress (USS), Poisson's ratio, creep strain rates,
Endurance limits, ect...... This information is of significant
importance to me and I look forward to what ever input you can provide
me with. Sincerely.................Paul Brown

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2