Don't forget anodizing (10um standard) is quite effective insulation ; not
quite the esd application .
Paul
> -----Original Message-----
> From: Windows/Admin/RLeckfor On Behalf Of Ronald J. Leckfor
> Sent: Tuesday, June 08, 1999 1:06 AM
> To: [log in to unmask]
> Subject: RE: [TN] ESD Issues
>
> Besides the ESD aspect, the added benefit of making it out of aluminum, is
> that the fixtures will not wear out easily, if you have it anodized to
> harden the metal, once the machining is done, and the fit and tolerances
> are verified!
>
>
>
> ----Original Message-----
> From: McMonagle, Michael R. [SMTP:[log in to unmask]]
> Sent: Saturday, June 05, 1999 9:39 AM
> To: [log in to unmask]
> Subject: Re: [TN] ESD Issues
>
> Eric,
> You should spend the extra money and make the
> fixtures from
> aluminum, ESD safe acrylic or one of the many conductive
> composite
> materials. This will alleviate any concerns of your ESD
> engineer.
>
> Mike McMonagle
> PCA Process Engineering Supervisor
> K*Tec Electronics
> 1111 Gillingham Lane
> Sugar Land, TX 77478
> (281) 243-5639 Phone
> (281) 243-5539 Fax
> [log in to unmask]
>
> > -----Original Message-----
> > From: Eric Kalgren [SMTP:[log in to unmask]]
> > Sent: Friday, June 04, 1999 5:24 PM
> > To: [log in to unmask]
> > Subject: [TN] ESD Issues
> >
> > I am in the process of designing and building fixtures to
> aid our
> > assemblers when soldering. My questions is: Do these
> fixtures need to
> > be conductive? Our assembly area follows strict ESD
> procedures and
> > the ESD engineer thinks that the fixtures should be
> conductive to the
> > static dissapative mats we work on.
> >
> > Thanks for your input,
> >
> > Eric Kalgren
> > BFGoodrich
> > Aerospce
> > Data Systems Division
> >
> >
> ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC
> using LISTSERV
> > 1.8c
> >
> ################################################################
> > To subscribe/unsubscribe, send a message to
> [log in to unmask] with
> > following text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> >
> ################################################################
> > Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services"
> > section for additional information.
> > For technical support contact Hugo Scaramuzza at
> [log in to unmask] or
> > 847-509-9700 ext.312
> >
> ################################################################
>
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using
> LISTSERV 1.8c
>
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask]
> with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
>
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at
> [log in to unmask] or 847-509-9700 ext.312
>
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|