Jason,
Both of the following 2 sources are on TechNet (and located in the Midwest)
and I have used both over the years for different types of analyses:
Robisan Laboratories : [log in to unmask]
Contamination Studies Laboratory : [log in to unmask] or
[log in to unmask]
Typically, they will provide the coupons cleaned to a cleanliness level and
sealed in individual bags prior to receipt.
Good luck.
Steve Sauer
Xetron Corporation
Cincinnati, OH
-----Original Message-----
From: Jason Smith [mailto:[log in to unmask]]
Sent: Monday, June 07, 1999 1:15 PM
To: [log in to unmask]
Subject: Re: [TN] contact for test coupons?
Anyone have a contact for obtaining IPC B-24 and IPC B-25 test coupons
referenced in the IPC-TM650 and Bellcore.
Jason Smith
Lexmark Electronics
Process Materials Engineer
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|