We are using a similar part and use a blind 8 mil via with a 20mil pad in the center of the BGA pad going
down to the 3rd layer. This has been very helpful, and has not been as costly as we thought it would. We
have had better yields using this method.
Susan Clayton
VMI
Jim Dobbins wrote:
> We have a design that utilizes a 620 ball 1mm pitch bga(6 balls deep / 26
> balls
> wide).
> In the past our dispersion and routing via has been a 25 mil pad, 10 mil
> drill, 35 mil clearance. Our designs are dense and typically utilize
> 5mil traces/spaces. We are still using the 25 mil via as the general
> routing via but looking for recommendations/examples of what folks are using
> for dispersion on 1mm bga s.
> Thanks,
> Jim
>
> ---------------------
> Jim Dobbins
> Tel: (408) 530-4700 Front Desk
> Tel: (408) 530-4745 Direct Line
> Email: [log in to unmask]
>
> ################################################################
> DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE DesignerCouncil <your full name>
> To unsubscribe: SIGNOFF DesignerCouncil
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|