I have found a cleaning system which removes only copper oxide and does not
touch the underlying copper. So, if I start with clean copper and laminate
within 8 hours why would I need a conversion coating? Epoxy bonds well to
clean copper doesn't it (even if it is an "optical polish" surface)?