TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Raymond Klein <[log in to unmask]>
Date:
Tue, 18 May 1999 17:10:35 -0700
Content-Type:
text/plain; charset="us-ascii"
X-To:
"[log in to unmask]"@gemini.adnc.com
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Raymond Klein <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Guys,

We are laying out a board for ICT and need to provide .030 inch dia. test
points on a .050 inch grid. The assembly/test shop is willing to accept a
.012 inch hole (somewhere) in the middle of the test point. Unfortunately
this board has a wave solder pass. My questions are:

1. Will flux get trapped underneath the solder mask over the via on the
board top (tented)? Is trapped flux a problem (the assemble uses organic
acidic flux)? short term?  long term?

2. If we un-mask the via on the top will I get solder balls popping through
the via holes?

3. Some of the vias are under SMT parts such as 56TSSOP that have very
little clearance above the board. Will the flux that gets through the
un-masked vias be adequately washed away in the water jet cleaning cycle?

Any advice in this matter is appreciated. Thank you in advance for benefit
of your experiences.

Ray Klein    [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2