Mornin' Steve -
You're right!!! But there's another way to work this thing -
Most important, stay out of the cleaning system - as others have pointed out,
the cleaning system will do more to damage the coating than everything else.
Second most important, don't use a no clean flux, unless you can be absolutely
sure that all of the material reacts to the heat of soldering (which I doubt
in a small rework situation).
Try the following:
Desolder and remove the parts - use no additive flux;
Scrub the affected area with a swab and a bit of 2-propanol to remove the
coating residues;
Pretin the new part, so it is as solderable as possible;
Solder new part, either using no flux or with a tiny bit of RMA flux;
Scrub the affected area with an acid brush and a bit of 2-propanol;
Dry the board - a brief pass thru an oven at 80-100C will get rid of all of
the surface moistures, etc.;
Patchcoat with a spray can of Humiseal 1B73, using a window mask cut from
teflon or similar sheet to limit the overspray. (This should be done rather
promptly after drying, when the board has cooled.)
Have a fun day guy - Kelly
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|