I believe the material they are specifying is Taconic's TLC-32-0310-CH/CH.
It is a PTFE/Glass material identified by the manufacturer as a low cost,
low dissipation, and tightly controlled dielectric. Try contacting :
Bruce Kline
Tel: 507-454-0097
Fax: 507-454-0098
e-mail: [log in to unmask] <mailto:[log in to unmask]>
for more information.
Jeffrey A. McGlaughlin
PCB Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]
-----Original Message-----
From: Neil Atkinson [SMTP:[log in to unmask]]
Sent: Friday, 14 May, 1999 07:17
To: [log in to unmask]
Subject: [TN] What the hell is this stuff??
We've just received a drawing that quotes a spec for laminate which
no one
seems to recognise, can anyone tell me what it is.
The material is quoted as: TLC TAC-LAM (32-0310-CH/CH) SUBSTRATE 31
THOU
THICK. DIELECTRIC CONSTANT 3.2 1/2 OZ ELECTRO-DEPOSITED COPPER BOTH
SIDES.
Thanks,
Neil
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|