We are having a problem with solder balls forming around
and in mounting holes that have been spot masked. The
problem seems to have surfaced after upgrading our Hollis
wave machine to use an Electrovert Lambda Wave Solder pot.
Other than the Solder balls forming, soldering quality is
very good.
Any Suggestions would be appreciated.
Flux - RMA thinned to Manufacturer's recommendations.
Spot Mask - Tech Spray Water Washable
Solder Temperature(SN63) - 500F
Top Board Temp before solder pot - 200F
Thanks
Virgil
----------------------
Virgil Lenton - Manufacturing Engineering
SED Systems Inc 18 Innovation Boulevard
P.O. Box 1464 Saskatoon, SK S7K 3P7
Ph. (306)931-3425 Fax (306)933-1486
Email:[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################