Hi Jack and all,
We like to add nonfunctional pads to a design for two reasons:
1). To prevent burning of isolated runs/pads when we pattern plate
2). On multilayer boards, we do it on inner layers to strengthen
the plated through holes
Hans
Air Force Material Command - We keep them flying!
~~~~~~~~
Hans M. Hinners WR-ALC/LYPME Bldg. 640
Materials Engineer 380 Second Street,
Suite 104
Manufacturing Eng. Sec. Robins AFB GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
[log in to unmask]
> It seems that most fabrication vendors prefer to remove the unconnected
> pads
> from inner-layers, in fact we do it for them before we send out the
> gerbers.
>
> But I thought I overheard Gary Ferrari say there was some test results
> that
> showed the board to be more reliable with all pads included, but I don't
> know where to find it or who did the testing.
>
> Does anyone know if it is significant enough to re-evaluate our process?
>
> Jack
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|