Steve
If I were faced with this the only questions I would have are:
- is it going to be inspectable? Is there sufficient gap for inspection
and to insure no CTE type interactions in the solder joints?
- if it is an SMT application, will it result in one joint being robbed of
solder (one joint has lots of solder, one joint doesn't have enough).
Dealt with a design once where several adjacent legs of a SOIC were
electrically common, the designer just put in one big pad instead of
electrically joined smaller ones. The net result was a lead in the middle
with lots of solder and the outside leads were "so so"...
- Graham Collins
-----Original Message-----
From: Tempea, Ioan [mailto:[log in to unmask]]
Sent: Friday, May 28, 1999 9:35 AM
To: [log in to unmask]
Subject: Re: [TN] assy: multiple terminations on 1 land
Steve,
we do this thing on most of our products.
Because of frequent ECOs, we have to alter a lot of assemblies and it is
pretty often that we connect two components on the same pad. And this is not
a production level solution, since the modifications are done according to
schematics issued by the Engineering.
Ioan
> -----Original Message-----
> From: Steve Quinn [SMTP:[log in to unmask]]
> Sent: Friday, May 28, 1999 8:14 AM
> To: [log in to unmask]
> Subject: [TN] assy: multiple terminations on 1 land
>
> hello all,
>
> I have been looking through the specs and have not been able to
> find
> anything saying it is a violation to have more than 1 part soldered to 1
> land. Is it OK to solder a 0603 component onto PLCC lands along with the
> PLCC.
> Thanks.
>
> Steve Quinn
>
>
>
> ===== ARTESYN TECHNOLOGIES - Communication Products Group ======
> ================================================================
>
> Steve Quinn Email: [log in to unmask]
> Process Engineer Phone: 608-831-5500
> 8310 Excelsior Drive Fax: 608-831-0872
> Madison, WI 53717
> =================================================================
> ====== Visit us at http://www.artesyn.com ======
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|