Wes Smith wrote regarding halogen free laminates.
In answer I think most laminators offer a halide free laminate. Two
which do are Isola and Mica-Micanite. Both in Europe.
As far as I know the material is UL 94V0
There is usually a long lead time and of course the price is higher.
For more information on flame retardants try:- www.bsef.com and
www.firesafety.org
> ----------
> From: Ian Boyton[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Ian Boyton
> Sent: 25 May 1999 11:19
> To: [log in to unmask]
> Subject: Re: [TN] Halogen Free PCB Materials
>
> Multicore produce colophony free solders in 3 and 5 core versions
> (reel).
> These have a halide content of 0.5% and conforms to j-std-004. However
> my
> own experience is that it is requires retraining to use and can leave
> a
> large flux deposit - unsightly but non corrosive. It's not perfect in
> my
> opinion but the world seems to be moving that way!
>
> Ian
>
> >From: Wes Smith <[log in to unmask]>
> >Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>, Wes
> Smith
> ><[log in to unmask]>
> >To: [log in to unmask]
> >Subject: [TN] Halogen Free PCB Materials
> >Date: Wed, 19 May 1999 08:48:46 +1000
> >MIME-Version: 1.0
> >From [log in to unmask] Tue May 18 15:55:47 1999
> >Received: from [208.150.51.11] by hotmail.com (1.5) with SMTP id
> >MHotMailB90B3AE1012FD820B648D096330B11831; Tue May 18 15:55:47 1999
> >Received: from jefry (208.150.51.11) by jefry.ipc.org (LSMTP for
> Windows NT
> >v1.1a) with SMTP id <[log in to unmask]>; Tue, 18 May 1999
> 17:41:34
> >-0500
> >Received: from JEFRY.IPC.ORG by JEFRY.IPC.ORG (LISTSERV-TCP/IP
> release
> >1.8c) with spool id 2018124 for [log in to unmask]; Tue,
> 18 May
> >1999 17:41:32 -0500
> >Received: from simon.ipc.org by jefry.ipc.org (LSMTP for Windows NT
> v1.1a)
> >with SMTP id <[log in to unmask]>; Tue, 18 May 1999
> 17:41:32
> >-0500
> >Received: from nsw-mail.acenet.com.au by simon.ipc.org via ESMTP
> >(951211.SGI.8.6.12.PATCH1502/940406.SGI) for <[log in to unmask]> id
> >RAA03602; Tue, 18 May 1999 17:31:06 -0700
> >Received: from wes_2 (bow-ppp153.acenet.com.au [203.35.156.53]) by
> >nsw-mail.acenet.com.au (8.9.2/8.9.2) with SMTP id IAA17950 for
> ><[log in to unmask]>; Wed, 19 May 1999 08:45:28 +1000 (EST)
> >X-Sender: [log in to unmask]
> >X-Mailer: Windows Eudora Pro Version 3.0 (32)
> >Message-ID: <[log in to unmask]>
> >Sender: TechNet <[log in to unmask]>
> >
> >Hi Folks,
> >
> >Can anybody point us in the right direction to find manufacturers of
> halide
> >free laminates, prepregs and solder mask materials. A search of
> "Dogpile"
> >(thanks Steve!) came up with plenty of cable manufacturers and
> reference to
> >a Toshiba patent in 1997, but nothing else.
> >
> >Is this "halide free PCB" requirement widespread or are we getting
> caught
> >up in the rush to "save" the planet?
> >
> >Assuming these materials are available, are they UL approved?
> >
> >Appreciate some input.
> >
> >Wes Smith.
> >
> >################################################################
> >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> >################################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> >text in the body:
> >To subscribe: SUBSCRIBE TechNet <your full name>
> >To unsubscribe: SIGNOFF TechNet
> >################################################################
> >Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section
> >for additional information.
> >For technical support contact Hugo Scaramuzza at [log in to unmask] or
> >847-509-9700 ext.312
> >################################################################
> >
>
>
> ______________________________________________________
> Get Your Private, Free Email at http://www.hotmail.com
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|