There are a few other things that I have seen to cause this.
If it is indeed a lead salt, a quick swab with household ammonia should remove it. If not, these
could be "freeze lines" caused by either contaminants in the solder (have you had it analyzed
recently?) or a more subtle defect caused by low antimony (possessing reverse TCE
characteristics).
Just my 2 cents worth,
Ed Popielarski
QTA Machine
10 Mc Laren, Suite D
Irvine, Ca. USA 92618
Ph: (949)581-6601
Fx: (949)581-2448
E-Mail: [log in to unmask]
http://www.qta.net
ASK ABOUT OUR BGA REBALLER!
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|