hi,
shore hardness is defined by an astm test method, the no. of which currently
escapes me. there is a shore 'A' for elastomers (read 'soft' things), and
there is a shore 'D' for harder things like plastics.
you use a durometer which has a dial gauge with a needle that you press into
the material you want to test. the depth of the penetration is indicated on
the dial gauge.
it is not used (as far as i know) to test the hardness of metals, ceramics,
etc.
phil crepeau
-----Original Message-----
From: Lautaro Gutierrez [mailto:[log in to unmask]]
Sent: Tuesday, May 25, 1999 7:53 PM
To: [log in to unmask]
Subject: [TN] Shore hardness
Please, send my a message if you know how does the shore harness method
works. I need inmformation urgent!
I must do a work: harness of different materials, any idea?
Thanks!!!!
_________________________________________________________
Do You Yahoo!?
Get your free @yahoo.com address at http://mail.yahoo.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|