I have seen the type of flux residues you describe a number of times. In
most cases, it has turned out to be a lead salt, for example lead adipinate
formed when adipic acid in the flux (an activator) react with lead oxide on
the surface to be soldered. My experience is that these salts are very
difficult to dissolve whatever solvent you use. Since the residues are so
difficult to dissolve, they are probably rather harmless for most
applications (but I have no proof for that statement). However, if you will
conformally coat the assemblies, they may cause poor adhesion of the
coating. What puzzle me is that you say it was manifested a few days after
aqueous wash. It should have been there immediately after cleaning.
Per-Erik Tegehall
IVF
Sweden
> ----------
>
> Has anyone ever come across white residues that looks like snow cap
> covering the solder joints? The phenomenon only manifested a few days
> after Aqueous wash and EDX captured high lead and oxygen. The white
> residues are so stubborn that they could not be dissolved in DI water and
> IPA. We use a water soluble paste and clean our assembly twice
>
> All inputs are welcome and appreciated.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|