Multicore produce colophony free solders in 3 and 5 core versions (reel).
These have a halide content of 0.5% and conforms to j-std-004. However my
own experience is that it is requires retraining to use and can leave a
large flux deposit - unsightly but non corrosive. It's not perfect in my
opinion but the world seems to be moving that way!
Ian
>From: Wes Smith <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>, Wes Smith
><[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Halogen Free PCB Materials
>Date: Wed, 19 May 1999 08:48:46 +1000
>MIME-Version: 1.0
>From [log in to unmask] Tue May 18 15:55:47 1999
>Received: from [208.150.51.11] by hotmail.com (1.5) with SMTP id
>MHotMailB90B3AE1012FD820B648D096330B11831; Tue May 18 15:55:47 1999
>Received: from jefry (208.150.51.11) by jefry.ipc.org (LSMTP for Windows NT
>v1.1a) with SMTP id <[log in to unmask]>; Tue, 18 May 1999 17:41:34
>-0500
>Received: from JEFRY.IPC.ORG by JEFRY.IPC.ORG (LISTSERV-TCP/IP release
>1.8c) with spool id 2018124 for [log in to unmask]; Tue, 18 May
>1999 17:41:32 -0500
>Received: from simon.ipc.org by jefry.ipc.org (LSMTP for Windows NT v1.1a)
>with SMTP id <[log in to unmask]>; Tue, 18 May 1999 17:41:32
>-0500
>Received: from nsw-mail.acenet.com.au by simon.ipc.org via ESMTP
>(951211.SGI.8.6.12.PATCH1502/940406.SGI) for <[log in to unmask]> id
>RAA03602; Tue, 18 May 1999 17:31:06 -0700
>Received: from wes_2 (bow-ppp153.acenet.com.au [203.35.156.53]) by
>nsw-mail.acenet.com.au (8.9.2/8.9.2) with SMTP id IAA17950 for
><[log in to unmask]>; Wed, 19 May 1999 08:45:28 +1000 (EST)
>X-Sender: [log in to unmask]
>X-Mailer: Windows Eudora Pro Version 3.0 (32)
>Message-ID: <[log in to unmask]>
>Sender: TechNet <[log in to unmask]>
>
>Hi Folks,
>
>Can anybody point us in the right direction to find manufacturers of halide
>free laminates, prepregs and solder mask materials. A search of "Dogpile"
>(thanks Steve!) came up with plenty of cable manufacturers and reference to
>a Toshiba patent in 1997, but nothing else.
>
>Is this "halide free PCB" requirement widespread or are we getting caught
>up in the rush to "save" the planet?
>
>Assuming these materials are available, are they UL approved?
>
>Appreciate some input.
>
>Wes Smith.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|