Hi Teo - The use of a vibrating mechanism on the reflow oven rail is a poor
substitute for fixing the real cause of skewed and shifted components! I
suggest focusing on why the components are being presented to the reflow
oven in a skewed position (poor placement?!) and solving that issue.
Vibrating a solder joint that is molten and/or in the process of
solidification can result in a number of solder joint wetting issues.
Dave Hillman
Rockwell Collins
[log in to unmask]
Teo Tijerina <[log in to unmask]> on 05/21/99 10:08:52 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
To: [log in to unmask]
cc:
Subject: [TN] vibrating mechanism on reflow oven rail
One of our supervisors attached a vibrating mechanism to the rail on the
reflow
oven. This helped align some skewed and shifted components. I have never
heard of this before. It appears to work, but there are some issues with
finding optimal frequencies, etc.
Is anyone using any technology similar to this?
-Teo Tijerina
Conexant Systems, Inc
El Paso, TX 79936
915.780.5552
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|