In a message dated 5/23/99 5:25:56 PM Pacific Daylight Time,
[log in to unmask] writes:
> While we're on the 20 mil subject ;
> the same apply on the polyimide ? ; as they have better release ratio than
> SS ?
> Any comments on plastic stencils in general ?
>
> Thanks paul
>
Hi ya' Paul!
First I gotta' tell ya', I sure do got some leads now after your
"unauthorized" post last week...I should say thanks. So; "thanks mate".
Now on to the technical stuff. I've never used a polyimide stencil, but I've
heard they're slick as snot...being able to see through them makes it really
easy to align when you're doing epoxy on the bottomside. I think I remember
Kathy Palumbo from Viking said she was using them and if I remember right she
said she liked them quite a bit. Heard they gasket really good so they reduce
the cleaning between prints quite a bit. Like to try one myself actually...
As far as how thick, I went to a Canadian company's WEB page that makes the
stencils and they recommend 5-mils for 20-mil pitch...a mil less than what
you would use for a stainless stencil. Their page is at:
http://www.kjmarketing.com
Say, what you asking 'bout stencils for anyway? Your Camelots breaking down
or something?
-Steve Gregory-
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|