hi,
it seems to me that this is a very benign thermal environment for compliant
pins. i don't know which vendor you are using, but i know that the vendors
that we deal with, teradyne and amphenol-bendix, have the data you need. it
is very important that you use the design guidelines that the vendor gives
you in order to assure the durability of the interconnection.
phil crepeau
-----Original Message-----
From: Elaine Gamboa [mailto:[log in to unmask]]
Sent: Wednesday, May 19, 1999 7:19 AM
To: [log in to unmask]
Subject: [TN] reliability testing on compliant pin technology
We perform environmental stress screening (-15 to 60 deg C) on our boards
and was wondering ifanyone know of some tests out there that prove compliant
pins would work in this type of process. Thanks.
EG
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|