Are these boards HASL? You may want to look to see if the coating is thicker on the one board. Without
knowing anything else that is the only thing I can think of at the moment which would cause a difference..
Hope this helps,
Rob Watson
Sanmina Corp.
Poh Kong Hui wrote:
> Hi,
>
> Have anyone encountered that PCB from different suppliers give different
> paste height.
>
> We are using 3 PCB suppliers for one of our product, and the average paste
> height we are getting (on 2 suppliers), using 6 mil stencil with rubber
> squeegee (70 durometer) gives an average paste height of 6.5 mil. However,
> there is one supplier's PCB that gives the average paste of 8 mil.
>
> We need to double the squeegee pressure to achieve the paste height of near
> 7.0 mil
>
> Could anyone advise me the cause to such issue.
>
> Thanks
>
> Poh
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|