Hi;
Today I find a catalog from a local representative of ERSA company, they
have a wave soldering machine named SO-NO-CLEAN that is fluxless and using
ultrasonics into the solder wave ( 20 KHz ) inside a sealed n2 chamber. So
the ability to make hundreds of solder joints is now available. The strange
thing is their web site don`t mention anything about that ...
http://www.ersa.de/emach_e.htm
Jorge Dourado de Santana
Maintenance / Process Engr
Microtec - Brazil
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: 8 de Maio de 1999 06:35
> To: [log in to unmask]
> Subject: Re: [TN] (Fwd) Ultrasonic soldering
>
> In a message dated 07/05/99 07:28:01AM, [log in to unmask]
> writes:
>
> My cynical two penneth:
> Interesting articles appear every few years putting forward ultrasonic
> soldering....
> but it never seems to go anywhere.
> Less cynically:
> I think possibly this is not because it doesn't work, but because it does
> away with the main advantage of the soldering process which is its ability
> to
> make hundreds of joints similtaneously. Where u/s is used industrially for
> joining it seems to be in welding where joints are made individually,
> these
> range from applications like wirebonding to joining plastics.
>
> Mike Fenner
> ..............
> > Hello all,
> >
> > I have just been reading an article on Ultrasonic soldering
> > which looks interesting, has anyone out there had had any
> > experience of this process?
> >
> > Thanks,
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|