Hi All,
I am looking for any information concerning the reduction of
tombstoning.
The only parameters that we can adjust are the size of the paste
dot, the type of paste used (any composition as long as it is eutectic
PB/SN), and the reflow profile (two atmosphere choices).
Since the physical pheomeonon is centered around surface tension I
am very interested to read about any study that was done that resulted in
reduced surface tension.
Currently the process is in the fractional percentages, the goal
is to go below 100 DPM.
Thanks,
Paul Gill
Process Engineer
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|