Dear Francis,

The "behavior" of tin-lead plating solutions with respect to cathode current
densities is generally to favor tin deposition over lead with increasing
cathode current densities. You may want to monitor your alloy across the
panel should you make any major changes in your plating current density.
        -----Original Message-----
        From:   Francis Lai [SMTP:[log in to unmask]]
        Sent:   Wednesday, March 31, 1999 8:02 PM
        To:     [log in to unmask]
        Subject:        [TN] Change in current densities in a Macdermid
Tin-lead bath

        I used current density 15mA/cm**2 in our Macdermid tin-lead bath for
5
        min. and I got 110 uin. with a 67% tin. But when I change the
current
        densities to 7.5mA/cm**2, I got 140 uin. with a 75% of tinfor 10
min..
        My question is will a change in current densities in a Macdermid
        tin-lead bath screw up the composition of Tin and Lead?
        My e-mail : [log in to unmask]

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
        For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
        ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2