Dan:

Electroply, a small laminate manufacturer may be able to help.  I think they are located in Southern
California and can be reached at 800-457-2557 or 310-322-5647.  Their web site is
http://www.electroply.com

Regards,

Ralph Richart
ICPC Etched Circuits

Dan Brandler wrote:

> Hello,
>
> We have a need for thin core ( .006" to .008")  FR-4
> laminate that's transparent to UV light. Our current
> suppliers only produce laminate with a UV block, adding
> dyes or multi-functional resin to their Fr-4 resin
> formulation.
>
> Does anyone know a source for "old fashioned" FR-4
> di-functional laminate without the UV block (i.e. white not
> yellow)? Please advise.
>
> Thank you, Dan Brandler, Ohmega technologies, Inc.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2