Ed: Your anxieties about the reliability of the connections you describe are
well founded. IMHO about the only chance for survival the circuits have, and
a slim one at that, is if the components (ceramic is assumed) are mounted to
a ceramic/alumina board (to negate or minimize Tce between component and
board). It would also aid reliability if the components have good standoff
above the board (>0.005 inch) so that sufficient solder pedestal exists to
provide some compliance. I am away from my office (in snowy Colorado) and
consequently don't have access to my files so am unable to reference you
directly to the appropriate technical information. You might review any work
by Manko, Zaro, etc., or wait for an input from Werner. Tread cautiously,
and make sure the method and results of any ESS are heeded.
Jim Moffitt
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|