This sounds right to me also, however, if your doing COB, I've found
that 6-10 micro inches works better, especially if in mass qtys such as
10k a month.
Scott
IDS
Meehan, Alexis wrote:
>
> We will be gold-plating some of our PCB's, and our manufacturing department
> has requested that
> we put this note on the fab drawings:
>
> Plating: Land will be 3 to 8 microinches gold immersion over 100-150
> microinches of electroless
> nickel over base metal.
>
> Do these thicknesses look right? Some folks in the company are questioning
> whether this is
> standard for most fab houses. Thanks in advance for any insight.
>
> *******************************************************
> Alexis Meehan Wavespan Corporation
> Mgr Engineering Srvs 500 N. Bernardo Avenue
> Tel: 650-237-8365 Mountain View, CA 94043
> Fax: 650-919-0191 http://www.wavespan.com
> ********************************************************
>
> ################################################################
> DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE DesignerCouncil <your full name>
> To unsubscribe: SIGNOFF DesignerCouncil
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|