We will be gold-plating some of our PCB's, and our manufacturing department
has requested that
we put this note on the fab drawings:
Plating: Land will be 3 to 8 microinches gold immersion over 100-150
microinches of electroless
nickel over base metal.
Do these thicknesses look right? Some folks in the company are questioning
whether this is
standard for most fab houses. Thanks in advance for any insight.
*******************************************************
Alexis Meehan Wavespan Corporation
Mgr Engineering Srvs 500 N. Bernardo Avenue
Tel: 650-237-8365 Mountain View, CA 94043
Fax: 650-919-0191 http://www.wavespan.com
********************************************************
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|