Has anyone heard of rosin based fluxes causing corrosion?
It is on a connector with solder cup connections and the flux used is
a RA flux. The pins and the solder is showing signs of corrosion.
Could this be caused or accelerated by the flux?
Any help is appreciated.
Ryan
-----------------------