As everyone may try to recover the solution of gold drag out bath which is
immediately followed by gold plating bath.
I am thinking about options like electrowinning, carbon absorption or even
concentrated it and put the solution back to the gold bath. Do you have
this experience and I desperately look for your input.
################################################################